Yet another body filler question. [Archive] - Chevelle Tech

: Yet another body filler question.


Randy Mosier
Mar 5th, 04, 9:23 AM
The repair job on the floor pan is done, but it has left the underside of the floor a bit on the rough side. It's smoother than the picture shows, but it could still use some sort of filler to help it blend in with the surrounding metal. The first picture is from the bottom, the second is the finished product on the inside of the car. What filler would be best for the underside of the floor, and what's the best way to go about filling and priming to keep rust away from the repair?

http://www.chevelles.com/showroom/Dcp_1808.jpg

http://www.chevelles.com/showroom/Dcp_1807.jpg

WayneK
Mar 5th, 04, 5:07 PM
Randy.. My .IMO use a Fiberglass Filler in your weld seams.. Kitty Hair is easy'er to work with then Gorlia Hair.. But both will do the trick for you..

For what it's worth ,I put fiberglass filer over ALL my welded seams..

Randy Mosier
Mar 6th, 04, 1:04 AM
I've got some Dynaglas out in the garage. Will that do the trick?

WayneK
Mar 8th, 04, 7:55 AM
sorry for the sloooooooow reply ( I was away all weekend) Yes I think ( ASSUME)that's just anothers CO's brand name...